Very interesting!

/ Very interesting! #2  
Pretty cool! Ive seen it done before, but never tested like that. Im impressed!
 
/ Very interesting! #3  
I am curious about the grade of aluminum. It says 3003. I wonder if this will work as well on other grades. I would like to know what he is using for flux and filler wire. It looks like this process is more foregiving than tiging thin aluminum.
Bill
 
/ Very interesting!
  • Thread Starter
#6  
I would like to know what he is using for flux and filler wire.
A member on another site seems to think the flux is borax dissolved in water. But he is going to do a little more research. Seems as I remember him using 1100-series Mig wire.
 

Marketplace Items

2017 Chevrolet Express 3500 12FT Box Truck w/ Liftgate (A61573)
2017 Chevrolet...
Freightliner Columbia (A63689)
Freightliner...
UNUSED WOLVERINE 6' FORK EXTENSIONS (A64281)
UNUSED WOLVERINE...
78in Bucket Skid Steer Attachment (A61572)
78in Bucket Skid...
YALE FORKLIFT (A63291)
YALE FORKLIFT (A63291)
2023 ASV RT-25 Posi-Track Compact Track Loader Skid Steer (A61572)
2023 ASV RT-25...
 
Top