Very interesting!

/ Very interesting! #2  
Pretty cool! Ive seen it done before, but never tested like that. Im impressed!
 
/ Very interesting! #3  
I am curious about the grade of aluminum. It says 3003. I wonder if this will work as well on other grades. I would like to know what he is using for flux and filler wire. It looks like this process is more foregiving than tiging thin aluminum.
Bill
 
/ Very interesting!
  • Thread Starter
#6  
I would like to know what he is using for flux and filler wire.
A member on another site seems to think the flux is borax dissolved in water. But he is going to do a little more research. Seems as I remember him using 1100-series Mig wire.
 

Marketplace Items

2009 Toyota Camry Hybrid Sedan (A61574)
2009 Toyota Camry...
2022 EZ-GO ELITE ELECTRIC GOLF CART (A63276)
2022 EZ-GO ELITE...
2020 INTERNATIONAL LT625 SLEEPER (A59911)
2020 INTERNATIONAL...
2017 NISSAN NV2500 4x2 VAN (A59911)
2017 NISSAN NV2500...
2018 International WorkStar 7500 T/A Matador 4,500 Gallon Septic Wet Vacuum Truck (A61573)
2018 International...
10' Dozer Blade (A64119)
10' Dozer Blade...
 
Top