Shield Arc
Super Member
Does he start the arc on the filler rod? A lot of guys who do top quality code work with scratch start Tig rigs do that. Lowers the risk of arc marks out side the weld zone, which is a big no, no! :thumbdown:
It was at 3:40. That was the Perfect video. Wish I saw that before I started learning.
More than a chuckle here... i dang near snorted a swig of Coke all over my keyboard. :laughing::laughing:I will have to admit that brought on a chuckle, and it CAN be just like that if your tungsten gets stuck, but with some practice it can be a lot easier than that.
This is great stuff! Why did I wait so long to get the TIG running? Probably because the only other time I tried it was Aluminum, and I had terrible trouble with contamination, and nobody to help me thru it. Was NOT very satisfying. This was a long time ago (before YouTube).
Here's a 1/2" extension bolt welded into a bung. Some fellers can probably tell what caused 'bobble' in the weld.
![]()