Why is that Mark, is the ER70S-6 stronger? Seems like I was looking for -6 but had to settle for -2.
 
   / Tig break test. #13  
70 S-6 seems to wet in better, and has a high level of deoxidizers. And in my experience is fairly ductile.
 
   / Tig break test. #14  
That's because you're better than me! :thumbsup:

I doubt that. If I came off sounding arrogant I apologize.:ashamed:
I don't even have any formal training. I pretty much taught myself what I know and that isn't saying much.
What you're saying is a 1/4" weld is probably a correct weld,compared to what I would think it is.

what amperage are you using, what kind of tungsten, and what gas. (argon or helium)

deereman75
I use a Lincoln Idealarc 300 AC/DC,not sure of the year,but I think it's from the late 80's early 90's.
When I weld 1/4 inch plate,I have it set on high,36/215,but I have the fine control on about 7.5,so I'm not using the full amps. I use 3/32" 2% Thoriated, "red" and 1/16" ER70S-2 rod (in fact the 70S is all we've ever bought).Gas is 100% Argon.

Greg
 
   / Tig break test. #15  
I doubt that. If I came off sounding arrogant I apologize.:ashamed:
I don't even have any formal training. I pretty much taught myself what I know and that isn't saying much.
What you're saying is a 1/4" weld is probably a correct weld,compared to what I would think it is.



deereman75
I use a Lincoln Idealarc 300 AC/DC,not sure of the year,but I think it's from the late 80's early 90's.
When I weld 1/4 inch plate,I have it set on high,36/215,but I have the fine control on about 7.5,so I'm not using the full amps. I use 3/32" 2% Thoriated, "red" and 1/16" ER70S-2 rod (in fact the 70S is all we've ever bought).Gas is 100% Argon.

Greg

Ahh the classic lincoln idealarc, oh how I wish I had one of those.
 
   / Tig break test. #16  
I saw you can buy tungsten in 7 inch lengths, I am wondering how you cut them, isnt tungsten incredibly hard?
 
   / Tig break test. #17  
I saw you can buy tungsten in 7 inch lengths, I am wondering how you cut them, isnt tungsten incredibly hard?

score it with a grinder and it will snap with minimum pressure.
 
   / Tig break test.
  • Thread Starter
#18  
What I do is put them 45 degrees to the outside edge of my bench grinder wheel, grind a groove in the tungsten, then break it over the edge of the table. Then grind the desired point on each end.
 
   / Tig break test. #19  
Ahh ok that makes sence. Also how much differnt is tig welding from gas welding, like if I am good at gas welding, how hard would it be to get good at tig welding.
 
   / Tig break test.
  • Thread Starter
#20  
They say the fastest way to learn Tig is to start with O/A. I haven't done any O/A welding in just under 100-years:laughing:, so I can't hardly remember what it's all about. I do remember it being very hot.
The similarities of the two processes are, forming the puddle, then dipping the filler. Personally I think Tig welding is easier to make a nice looking bead.
 

Attachments

  • drain plug 2.jpg
    drain plug 2.jpg
    97 KB · Views: 220

Tractor & Equipment Auctions

2007 Pace American Enclosed Trailer (A49461)
2007 Pace American...
2011 Ford Flex SUV (A50860)
2011 Ford Flex SUV...
2005 International Pier Drilling Truck (A49461)
2005 International...
Willmar 4300 Wrangler Loader (A51039)
Willmar 4300...
30ft Pole S/A Towable Trailer (A49346)
30ft Pole S/A...
2025 K1912 UNUSED Metal Livestock Shed (A50860)
2025 K1912 UNUSED...
 
Top