City Farmer
Platinum Member
- Joined
- Jan 3, 2013
- Messages
- 528
- Location
- Chesterfield, Mi
- Tractor
- Ford 3000, 4400 & 4500TLB Case 830 Case 350 dozer
I put together a scratch start tig for my Miller thunderbolt ac/dc stick welder today. These are my first and second beads with a tig torch. I'm using 100% argon set at 15. It seems to run ok once it gets hot but the tungsten gets worn out really quick. Any tips for that? Here's a couple pictures. Any tips or recommendations would be appreciated. The second & third picture are the front and back of the same weld, I never welded the back side. I think there was to much heat to make it blow through like that.